1 | 30439045-NC.pdf |
3 | 117_203e_CD.pdf 117_203e_CD (1).pdf |
4 | IEC+62862-3-6+ED1-CD-1-en.pdf |
6 | FOREWORD |
8 | 1 Scope 2 Normative references |
9 | 3 Terms and definitions 3.1 General definitions 3.2 Optical properties |
10 | 3.3 Environmental parameters 3.4 Corrosion parameters |
11 | 4 Samples 4.1 Sampling 4.2 Sample preparation |
13 | 4.3 Placement of samples in corrosion test chambers |
14 | 4.4 Post-test sample treatment 5 Sample characterization 5.1 General remarks 5.2 Visual Inspection |
15 | 5.3 Measurement of reflectance 5.3.1 Hemispherical reflectance 5.3.2 Near-normal monochromatic specular reflectance 5.4 Measurement of inner corroded area (optional) |
17 | 6 Test method and assessment 6.1 Overview of test procedure |
19 | 6.2 Assessment |
20 | 7 Accelerated aging test procedures 7.1 General remarks 7.2 Neutral salt spray test (NSS) |
21 | 7.3 Copper Accelerated Acetic Acid Salt Spray test (CASS) |
22 | 7.4 Condensation test (COND) 7.5 Thermal Cycling / Humidity test (TCH) |
23 | 7.6 Damp Heat test (DH) |
24 | 7.7 UV / Humidity test (UVH) |
25 | 7.8 Abrasion test (ABR) |
26 | 7.9 Sand Erosion test (SE) 8 Reporting 8.1 General information |
27 | 8.2 Methodology |
28 | 8.3 Results 8.4 Conclusions |
29 | Annex A Testing of reflector types of different composition informative |
30 | Annex B Estimation of degradation in outdoor environment informative B.1 Estimation of erosion in different outdoor environments B.2 Estimation of corrosion in different outdoor environments |
31 | B.3 Estimation of overall degradation |