BS EN 13603. Copper and copper alloys. Test methods for assessing protective tin coatings on drawn round copper wire for electrical purposes

Published By Publication Date Number of Pages
BSI 2020 24
Guaranteed Safe Checkout
Categories: ,

If you have any questions, feel free to reach out to our online customer service team by clicking on the bottom right corner. We’re here to assist you 24/7.
Email:[email protected]

This document specifies methods for assessing the tin coating on drawn round copper wire for the manufacture of electrical conductors, e.g. according to EN 13602.

This document includes test methods for the determination of the following characteristics:

  1. thickness of the unalloyed tin coating;

  2. continuity of the tin coating;

  3. adherence of the tin coating.

WARNING — This document can involve the use of hazardous materials, operations, and equipment. This document does not purport to address all of the safety problems associated with their use. It is the responsibility of the user of this document to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. Moreover this document does not cover the aspects related to the people protection against the X-ray. To obtain information applicable to this aspect it is convenient to refer to national and international standards, and also to the local regulations if they exist.

PDF Catalog

PDF Pages PDF Title
6 1 Scope
2 Normative references
3 Terms and definitions
7 4 Thickness of the unalloyed tin coating
4.1 Principle of the method based on the electrolytic dissolution of the tin coating
4.1.1 General
4.1.2 Reagents and materials
4.1.3 Apparatus
4.1.3.1 Direct reading instruments
8 4.1.3.2 Other instruments
4.1.3.3 Electrolytic cell
9 4.1.4 Preparation of the test piece
4.1.5 Procedure for determining the thickness of unalloyed tin coatings
4.1.5.1 General
4.1.5.2 Determination of measuring area
4.1.5.3 Electrolysis (Dissolution of the unalloyed tin coating)
4.1.5.4 Factors affecting the measuring accuracy
10 4.1.5.5 Measurement uncertainty
11 4.1.5.6 Determination of electrolyte efficiency
12 4.1.6 Expression of results
4.2 Principle of the method based on XRF
4.2.1 General
13 4.2.2 Devices with measuring spots larger than the wire diameter – Overlap technique
14 4.2.3 Devices with measuring spots smaller than the wire diameter – Full-spot technique
4.2.4 Preparation of the test piece
4.2.5 Factors affecting the measuring accuracy
19 5 Continuity of the tin coating
5.1 Principle
5.2 Test solution
5.3 Reference solution
20 5.4 Preparation of the test piece
5.5 Cleaning of the test piece
5.6 Immersion for testing
5.7 Determination
5.7.1 General
21 5.7.2 Comparison by Nessler cylinders
5.7.3 Colorimetric method
6 Adherence of the tin coating
6.1 Principle
6.2 Stock solution
6.3 Test solution
6.4 Preparation of the test piece
22 6.5 Cleaning of the test piece
6.6 Immersion for testing
6.7 Examination
23 7 Test report
BSI 20/30396895 DC 2020